EXTERIOR VARNISH TECHNOLOGY
Apply one coat of stain SX104 (or impregnant ED4405 for coniferous wood, ED4404 for deciduous wood), then wait for it to dry for about 1 hour at 20C.
Apply one coat of varnish EM1472-0030 tinted with 10% stain SX104 (drying about 3 hours at 20C)
After the nail dries, intermediate sanding is done with an abrasive sponge or sandpaper with P220 grain
Apply second-hand varnish EM1472-0030 tinted with 10% stain SX104
The varnish dries completely after 6-8 hours at 20C.
(When the wood should remain natural color, apply one coat of impregnated ED4404 or ED4405 instead of SX104 stain)
Consumption rate: